JY·A102 Titanium calcium type coating Cr19Ni10 stainless steel elektroda
Tujuan:Digunakake kanggo welding struktur baja tahan karat tahan karat, kayata 06Cr19Ni10 lan 06Cr18Ni¹1Ti lan suhu apa sing kudu ngisor 300 ℃



Item Tes | C | Mn | Si | S | P | Cr | Ni | Mo | Cu |
Nilai njamin | ≤0.08 | 0,50-2,50 | ≤1.00 | ≤0,030 | ≤0,040 | 18.0-21.0 | 9.0~11.0 | ≤0,75 | ≤0,75 |
Hasil Umum | 0.041 | 1.35 | 0.69 | 0.008 | 0,022 | 19.5 | 9.6 | 0.064 | 0.1 |
Item Tes | Rm (MPa) | A(%) |
Nilai njamin | ≥550 | 30 |
Hasil Umum | 600 | 42 |
Dhiameter (mm) | φ2.0 | φ2.5 | φ3.2 | Φ4.0 | φ5.0 |
Ampere (A) | 40~80 | 50~100 | 70~130 | 100~160 | 140~200 |
Cathetan: 1.Elektroda kudu dipanasake ing suhu 300 ° C sajrone 1 jam. Preheat rod kapan wae digunakake
2.Preferred sumber daya DC,arus listrik ngirim ora dhuwur.
Tulis pesen sampeyan ing kene lan kirimake menyang kita